** Soak till even temperature
** Cool as slowly as possible, either in vermiculite or in the furnace
** Some steels have a thermal "no-go" zone where you can't linger, check the datasheet
** Results in a soft steel that's cold-workable
* Normalizing
Line 113 ⟶ 114:
|| Knowing the serious errors and how to avoid them
|}
 
== Practical Forging ==