* Parameters set using the middle section. We're using DC (Electrode negative), no pulse, HF-TIG in 2T mode. Back and Forward controls step through the parameters that are relevant to the selected mode
** Using the chart on top of the welder to pick settings
** If the chart isn't helping then use the following guidelines. Use all the %age changes that apply to your work, e.g. if you're doing an insideoutside corner on stainless steel then apply both -%10 current for Stainless and -10% current for outside corner for a total of -20% change to current and +45% gas
{| class="wikitable"
|-